A.3 Other Notes
1) Printer mechanism handling
Do not pull the paper out when the cover is closed.
Because the thermal elements of the print head and driver IC are easy to break, do not
touch them with any metal objects.
Since the areas around the print head become very hot during and just after printing, do not
touch them.
Do not use the cover open button except when necessary, since the printer mechanism
may be damaged.
Do not touch the surface of the print head because dust and dirt can stick to the surface and
damage the elements.
Thermal paper containing a great deal of Na
+
, K
+
, and Cl
-
ions can harm the print head
thermal elements. Therefore, be sure to use only the specified paper.
2) Thermal paper handling
Notes on using thermal paper
Chemicals and oil on thermal paper may cause discoloration and faded printing.
Therefore, pay attention to the following:
a) Use water paste, starch paste, polyvinyl paste, or CMC paste when gluing thermal
paper.
b) Volatile organic solvents such as alcohol, ester, and ketone can cause discoloration.
c) Some adhesive tapes may cause discoloration or faded printing.
d) If thermal paper touches anything which includes phthalic acid ester plasticizer for a
long time, it can reduce the image formation ability of the paper and can cause the
printed image to fade. Therefore, when storing thermal paper in a card case or
sample notebook, be sure to use only products made from polyethylene,
polypropylene, or polyester.
e) If thermal paper touches diazo copy paper immediately after copying, the printed
surface may be discolored.
f) Thermal paper must not be stored with the printed surfaces against each other,
because the printing may be transferred between the surfaces.
g) If the surface of thermal paper is scratched with a hard metal object such as a nail,
the paper may become discolored.